[ 01 ] Every grade we document

Grade Finder

Search the full grade index by designation, standard, equivalent or application.

Download catalogue

Every grade we document

8 grades found

Cupro Nickel 90/10 Seamless Pipes

Cupro Nickel 90/10 Seamless Pipes

Mill indent
UNS C70600EN CW352H / CuNi10Fe1Mn

The default seawater alloy. 90% copper with 10% nickel and a controlled iron addition builds a protective cuprous oxide film in seawater, and the inherent copper toxicity stops macrofouling — barnacles and mussels do not settle, so cooling lines stay clean without chlorination. Specified for ship and platform seawater systems, firewater ring mains and condenser tubing where the velocity stays below about 3.5 m/s.

7 forms available
Cupro Nickel 70/30 Seamless Pipes

Cupro Nickel 70/30 Seamless Pipes

Mill indent
UNS C71500EN CW354H / CuNi30Mn1Fe

The higher-duty cupro nickel. Tripling the nickel to 30% raises strength, erosion-corrosion resistance and the allowable seawater velocity to around 4.5 m/s, and lifts the service temperature well above 90/10. It is the grade for pump and valve-adjacent piping, hot brine and MSF desalination heat recovery, and any line where turbulence or sand loading would strip the film off 90/10.

7 forms available
Cupro Nickel 66/30/2/2 (C71640)

Cupro Nickel 66/30/2/2 (C71640)

Project supply
UNS C71640EN CuNi30Fe2Mn2

The desalination variant of 70/30. Raising iron and manganese to about 2% each stabilises the protective film under high velocity, sand-laden and partly deaerated brine, which is exactly the duty inside MSF evaporator heat recovery and reject sections. Where 70/30 tubes thin at the inlet ends, C71640 holds.

4 forms available
Duplex 2205

Duplex 2205

Ex-stock Dubai
UNS S31803 / S32205EN 1.4462

The most widely used duplex grade. Roughly double the yield strength of 316L, allowing thinner and lighter sections while delivering far better chloride stress corrosion cracking resistance.

6 forms available
Super Duplex 2507

Super Duplex 2507

Mill indent
UNS S32750 / S32760EN 1.4410 / 1.4501

Super duplex with PREN above 40 for the most aggressive seawater and sour service. S32760 (Zeron 100) adds tungsten and copper for enhanced acid resistance.

5 forms available
316 / 316L

316 / 316L

Ex-stock Dubai
UNS S31600 / S31603EN 1.4401 / 1.4404

Molybdenum-bearing austenitic stainless steel. The 2-3% Mo addition transforms pitting resistance in chloride-bearing media, making 316L the baseline grade for marine and chemical service in the Gulf.

6 forms available
317L Stainless Steel

317L Stainless Steel

Mill indent
UNS S31703EN 1.4438 / X2CrNiMo18-15-4

A molybdenum-up step on 316L. Raising Mo to 3 - 4% lifts PREN to around 30, which buys real margin against pitting and crevice attack in pulp, scrubber and chloride service where 316L is borderline but duplex is more than the duty needs.

6 forms available
Titanium Grade 2

Titanium Grade 2

Mill indent
UNS R50400EN 3.7035

Commercially pure titanium, the industry workhorse. Fully resistant to seawater and oxidising chlorides with excellent formability and weldability.

6 forms available